dc.contributor.authorSalah Fadhil Abduljabbar-
dc.date.accessioned2023-10-22T08:41:42Z-
dc.date.available2023-10-22T08:41:42Z-
dc.date.issued2019-
dc.identifier.citationhttps://djes.info/index.php/djesen_US
dc.identifier.issn1999-8716-
dc.identifier.urihttp://148.72.244.84:8080/xmlui/handle/xmlui/5900-
dc.description.abstractPowder metallurgy technique utilized in samples preparing. Samples were compacted by using cold uniaxial pressing then followed by sintering process at 600 oC under inert gas. Results showed improving in (Brinell Hardness, wear resistance & compression strength) and increasing in (density, porosity & water absorption). Brinell Hardness increasing (106. – 114.7), compression strength increasing (35.1 – 40.8) N/mm2 and decrease wear rate (6.6*exp(-8) – 4.22*exp(-8)) g/cm at time 30 min. with (0 – 20)% Al2O3&B4C. While increase apparent density (2.76 – 2.83) g/cm3, Bulk Density increase (2.71-2.82) g/cm3 apparent porosity decrease (1.88 – 0.193) % and water absorption decrease (0.699 – 0.068) % at (0 – 20) % Al2O3&B4C.en_US
dc.language.isoenen_US
dc.publisherUniversity of Diyala – College of Engineeringen_US
dc.subjectComposite Materialsen_US
dc.subjectPowder Metallurgyen_US
dc.subjectAluminumen_US
dc.subjectPhysical Propertiesen_US
dc.subjectMechanical Propertiesen_US
dc.titleStudy of the Effect of Al2o3&B4c Particles Reinforcement on Some Physical and Mechanical Properties for Aluminum Alloy 6063 by Powder Metallurgy Techniqueen_US
dc.typeArticleen_US
Appears in Collections:مجلة ديالى للعلوم الهندسية / Diyala Journal of Engineering Sciences (DJES)

Files in This Item:
File Description SizeFormat 
551 5.pdf762.42 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.